Vopcrom DSA
A hard chrome procedure of the third generation. ... High current efficiency (18-25%)... Low anode corrosion ... No etching on steel and steel alloys. ... Bright deposits with good leveling. ... High deposit speed compared with standard process Good corrosion protection and wear resistance of the layer. Good micro cracking qualities (approx. 300 - 800 cracks/cm). Bright, hard chrome layers (approx. 800 – 1100 HV).... The hard chrome process for the future